CREEP TESTING MACHINE Deluxe

Need Help?
+91 98967 93832Applications
A sturdy bench-top mounted unit for studying the effect of creep on different material test specimens. Necked test specimens are held vertically in special clamps which do not induce bending during loading. A lever arm transmits load from a hanger and weights into the specimen; a counter-balance weight ensures the lever arm self-weight is calibrated out. Learn about CREEP TESTING MACHINE suppliers for optimal educational outcomes.. A transparent specimen guard surrounds the test specimen, allowing the surrounding temperature to be adjusted hot or cold, read using the supplied thermometer, and controlled using a special thermal pack. The cover also allows easy viewing of the specimen during creep. Learn about CREEP TESTING MACHINE exporters for optimal educational outcomes.. A dial gauge measures specimen extension throughout testing. Polypropylene specimens are supplied as standard. Learn about CREEP TESTING MACHINE strength-materials-hsm India for optimal educational outcomes.. Optional nylon and PVC specimen sets are also available. A full technical instruction manual is supplied. Learn about CREEP TESTING MACHINE for educational labs for optimal educational outcomes..
Technical Specifications
- Loading arm ratio: 4:1
- Polypropylene specimens: 10 per set
- Specimen: 22mm gauge length, 4.8(W) × 1.6(t) mm nominal
- Load hanger: 1N
- Dial gauge: 0.01mm resolution, 25mm travel
- Thermometer
- Transparent specimen cover
- Hot and cold packs
Similar Products